Tungsten electrode tig welidng rod
Chemical Composition:
Type | Substances | Added oxide % | Impurities content % | Tungsten % | Color sign |
WC20 | CeO2 | 1.8-2.0 | <0.20 | Remaining | Grey |
WL10 | La2O3 | 0.8-1.2 | <0.20 | Remaining | Black |
WL15 | La2O3 | 1.3-1.7 | <0.20 | Remaining | Golden yellow |
WL20 | La2O3 | 1.8-2.2 | <0.20 | Remaining | Sky blue |
WZ3 | ZrO2 | 0.2-0.4 | <0.20 | Remaining | Brown |
WZ8 | ZrO2 | 0.7-0.9 | <0.20 | Remaining | White |
WT10 | ThO2 | 0.9-1.2 | <0.20 | Remaining | Yellow |
WT20 | ThO2 | 1.7-2.2 | <0.20 | Remaining | Red |
WT30 | ThO2 | 2.8-3.2 | <0.20 | Remaining | Purple |
WT40 | ThO2 | 3.8-4.2 | <0.20 | Remaining | Orange |
WP | – | – | <0.20 | Remaining | Green |
WY20 | Y2O3 | 1.8-2.2 | <0.20 | Remaining | Blue |
WR | – | 1.2-2.5 | <0.20 | Remaining | Pink |
Size:
Diameter | Diameter tolerance | Length | Length tolerance | |
mm | inch | mm | mm | mm |
1 | 1/25 | (+/-)0.01 | 50,75,150,175 | (+/-)1.0 |
1.2 | 6/125 | (+/-)0.01 | 50,75,150,175 | (+/-)1.0 |
1.6 | 1/16 | (+/-)0.02 | 50,75,150,175 | (+/-)1.0 |
2 | 2/25 | (+/-)0.02 | 50,75,150,175 | (+/-)1.0 |
2.4 | 3/32 | (+/-)0.02 | 50,75,150,175 | (+/-)1.0 |
3 | 3/25 | (+/-)0.03 | 50,75,150,175 | (+/-)1.0 |
3.2 | 1/8 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
4 | 5/32 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
4.8 | 3/16 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
5 | 1/5 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
6 | 15/64 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
6.4 | 1/4 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
8 | 5/16 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
10 | 2/5 | (+/-)0.04 | 50,75,150,175 | (+/-)1.0 |
Note:When you need other tungsten wolfram electrodes, please send us the inquiry including
designation and length*diameter.
tungsten welding electrode:
1. It used when arc welding with the Tungsten Inert gas (TIG) process or when plasma welding.
2. In both processes the electrode, arc and weld pool are protected from atmospheric contamination by an inert gas.
3. It used because it can withstand very high temperatures with minimal melting or erosion.
4. it made by powder metallurgy and are formed to size after sintering.
Feature
• Low electronic function
• Good conductivity
• Good electron emission ability
• Good mechanical cutting performance
• High elastic modulus, Low vapour pressure
• High recrystallization temperature |
Product detail pictures:
Related Product Guide:
Travis Perkins PLC takes encouragement from improved trading | Pure Molybdenum Strip
Mohamed Salah hits hat-trick as Liverpool run riot at Bournemouth The Telegraph Search Icon Save Facebook icon Twitter icon Instagram icon LinkedIn icon Facebook icon Twitter icon Instagram icon LinkedIn icon | Slivery Color Molybdenum Sheet /Plate
We're committed to providing easy,time-saving and money-saving one-stop purchasing service of consumer for OEM China Molybdenum Heating Elements - WCE/WT/WP/WL/WZ tig welding rod tungsten electrode – Forged Tungsten , The product will supply to all over the world, such as: Nairobi , Rome , Vietnam , We have now a good reputation for stable quality goods, well received by customers at home and abroad. Our company would be guided by the idea of "Standing in Domestic Markets, Walking into International Markets". We sincerely hope that we could do business with car manufacturers, auto part buyers and the majority of colleagues both at home and abroad. We expect sincere cooperation and common development!
By Delia Pesina from Italy - 2018.11.11 19:52
This company has the idea of "better quality, lower processing costs, prices are more reasonable", so they have competitive product quality and price, that's the main reason we chose to cooperate.
By Flora from Ecuador - 2018.09.19 18:37